X2CrTi12 - 1.4512

X2CrTi12 - (1.4512) / S40900 / SUS409L / Z3CT12 / 409S

Application Information


Public Id

X2CrTi12 - 1.4512

Grade (EU) X2CrTi12
Number 1.4512
EU - EN X2CrTi12
USA S40900
France, AFNOR Z3CT12
England, BS 409S
Japan, JIS SUS409L


Classification

X2CrTi12 - 1.4512

EN 10088-2: 2005
EN 10296-2: 2005
EN 10297-2: 2005
EN 10088-1: 2005
EN 10088-4: 2009

Chemical Composition

X2CrTi12 - 1.4512

C max 0.03
Si max 1.00
Mn max 1.00
P max 0.04
S max 0.015
Cr 10.5 - 12.5
Ti max 0.65

Mechanical Properties

X2CrTi12 - 1.4512

Rm - Tensile strength (MPa) (+A) 380 - 560

X2CrTi12 - 1.4512

Rp0.2 0.2% proof strength (MPa) (+QT650) 210

X2CrTi12 - 1.4512

A - Min. elongation at fracture (%) (+A) 25

X2CrTi12 - 1.4512

Equivalent References

USA S40900
Japan, JIS SUS409L
France, AFNOR Z3CT12
England, BS 409S

Detailed Feature Table...

X6Cr13 - 1.4000

Equivalent References

USA S41008
Japan, JIS SUS410S
France, AFNOR Z6C13
England, BS 403S17

Detailed Feature Table...

X6Cr17 - 1.4016

Equivalent References

USA S43000
Japan, JIS SUS430
France, AFNOR Z8C17
England, BS 430S17

Detailed Feature Table...

X3CrTi17 - 1.4510

Equivalent References

USA S43035
Japan, JIS SUS430LX
France, AFNOR Z4CT17
Russia, GOST 08KH17T

Detailed Feature Table...